Nylon toughening agent SWR-3A
Key words:
Classification:
Description
Technical Index
Serial Number | Item | Index |
1 | Appearance | Natural color particles |
2 | Density (g/cm3) | 0.92±0.02 |
3 | Melt flow rate g/10min 190℃ 2.16kg 230℃, 5kg |
2.5-4 ≥12.0 |
4 | Grafting rate % | 0.8 |
Usage range:
Used for PA6 toughening, strengthening and toughening, improving the impact resistance, cold resistance, and moldability of nylon, and reducing water absorption.
Used as a compatibilizer for nylon and polypropylene/polyethylene blends.
Used as a macromolecular coupling agent for mineral and glass fiber filled nylon.
Used as a compatibilizing toughening agent for glass fiber or filler filled PP, with both compatibilizing and toughening effects.
Usage method:
Proportionally extruded and granulated by twin-screw extruder, or directly injection molded.
Reference Proportion:
Users should add according to their requirements and cost-effectiveness.
Storage:
20kg packaging, stored in a ventilated and dry place, not exceeding 24 months from the date of production.